General
Property | Temperature | Value |
---|---|---|
Absorción de agua | 23.0 °C | 0 % Show Supplier Material materials with Absorción de agua of 0 % |
Densidad | 23.0 °C | 2.92 g/cm³ Show Supplier Material materials with Densidad of 2.92 g/cm³ |
Tamaño de grano | 22 μm Show Supplier Material materials with Tamaño de grano of 22 μm |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.26 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.26 [-] |
Hardness, Rockwell Superficial 45-N | 23.0 °C | 60 [-] Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 60 [-] |
Módulo elástico | 23.0 °C | 345 GPa Show Supplier Material materials with Módulo elástico of 345 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 3.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.5 MPa·√m |
Resistencia a la compresión | 23.0 °C | 1.55 MPa Show Supplier Material materials with Resistencia a la compresión of 1.55 MPa |
Resistencia a la flexión | 23.0 °C | 207 MPa Show Supplier Material materials with Resistencia a la flexión of 207 MPa |
Resistencia a la tracción | 23.0 °C | 152 MPa Show Supplier Material materials with Resistencia a la tracción of 152 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 1046 J/(kg·K) Show Supplier Material materials with Calor específico of 1046 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 9E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9E-6 1/K |
Conductividad térmica | 23.0 °C | 325 W/(m·K) Show Supplier Material materials with Conductividad térmica of 325 W/(m·K) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 6.76 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 6.76 [-] | |
Dielectric constant, 10GHz | 23.0 °C | 6.76 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 6.76 [-] | |
Dissipation factor, 1MHz | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4E-4 [-] | |
Resistividad eléctrica | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+13 Ω·m | Minimum |
Rigidez dieléctrica | 23.0 °C | 0.23 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 0.23 kV/mm | AC, 6.35mm |
Technological properties
Property | ||
---|---|---|
Application areas | Diode lasers, Medical scanning equipment, Semiconductor substrates, Automotive ignition systems, Thick film circuits, Components for missile guidance, Radio frequency transmitters | |
Color | Light Grey |