Property | Temperature | Value |
---|---|---|
Absorción de agua | 23.0 °C | 0 % Show Supplier Material materials with Absorción de agua of 0 % |
Densidad | 23.0 °C | 3.95 g/cm³ Show Supplier Material materials with Densidad of 3.95 g/cm³ |
Tamaño de grano | 1 μm Show Supplier Material materials with Tamaño de grano of 1 μm |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.22 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.22 [-] |
Hardness, Rockwell Superficial 45-N | 23.0 °C | 85 [-] Show Supplier Material materials with Hardness, Rockwell Superficial 45-N of 85 [-] |
Módulo elástico | 23.0 °C | 375 GPa Show Supplier Material materials with Módulo elástico of 375 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m |
Resistencia a la compresión | 23.0 °C | 2.41 MPa Show Supplier Material materials with Resistencia a la compresión of 2.41 MPa |
Resistencia a la flexión | 23.0 °C | 379 MPa Show Supplier Material materials with Resistencia a la flexión of 379 MPa |
Resistencia a la tracción | 23.0 °C | 276 MPa Show Supplier Material materials with Resistencia a la tracción of 276 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 837.36 J/(kg·K) Show Supplier Material materials with Calor específico of 837.36 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 8E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8E-6 1/K | RT to 1000°C |
Conductividad térmica | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Conductividad térmica of 35 W/(m·K) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 9.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 9.7 [-] | |
Dielectric constant, 10GHz | 23.0 °C | 9.6 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 9.6 [-] | |
Dissipation factor, 1MHz | 23.0 °C | 1E-4 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1E-4 [-] | |
Resistividad eléctrica | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+13 Ω·m | Minimum |
Rigidez dieléctrica | 23.0 °C | 0.22 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 0.22 kV/mm | AC, 6.35mm |
Technological properties
Property | ||
---|---|---|
Application areas | photonics/ lasers, defense, energy, telecommunications and semiconductor manufacturing | |
Color | White |