General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.81 g/cm³ Show Supplier Material materials with Densidad of 8.81 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1.27 - 406.5 mm Show Supplier Material materials with Ancho of 1.27 - 406.5 mm |
Espesor | 0.05 - 2.03 mm Show Supplier Material materials with Espesor of 0.05 - 2.03 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 720 - 860 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 720 - 860 MPa |
Módulo elástico | 23.0 °C | 135 GPa Show Supplier Material materials with Módulo elástico of 135 GPa |
Plegabilidad 90 ° bidireccional | 23.0 °C | 1.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1.5 [-] |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 1.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1.5 [-] |
Resistencia a la tracción | 23.0 °C | 825 - 965 MPa Show Supplier Material materials with Resistencia a la tracción of 825 - 965 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 221 W/(m·K) Show Supplier Material materials with Conductividad térmica of 221 W/(m·K) |
Eléctrico
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 50 % IACS Show Supplier Material materials with Specific Electrical conductivity of 50 % IACS | nominal value |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Berilio | 0.15 - 0.5 % Show Supplier Material materials with Berilio of 0.15 - 0.5 % | ||
Circonio | 0.5 % Show Supplier Material materials with Circonio of 0.5 % | max. | |
Cobre | Balance | ||
Estaño | 0.25 % Show Supplier Material materials with Estaño of 0.25 % | max. | |
Níquel | 1 - 1.4 % Show Supplier Material materials with Níquel of 1 - 1.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Brush 60 was performance engineered for electronic contact and spring applications in the computer, datacom and telecommunications markets. |