General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.81 g/cm³ Show Supplier Material materials with Densidad of 8.81 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1.27 - 406.5 mm Show Supplier Material materials with Ancho of 1.27 - 406.5 mm |
Espesor | 0.05 - 0.38 mm Show Supplier Material materials with Espesor of 0.05 - 0.38 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 280 - 340 [-] Show Supplier Material materials with Dureza Vickers of 280 - 340 [-] | |
Elongación | 23.0 °C | 1 % Show Supplier Material materials with Elongación of 1 % | in 25mm |
Límite elástico Rp 0,2 | 23.0 °C | 930 - 1055 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 930 - 1055 MPa | |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 5 [-] | >10mm (2 for <10mm) |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 5 [-] | >10mm (2 for <10mm) |
Resistencia a la fatiga | 23.0 °C | 580 - 685 MPa Show Supplier Material materials with Resistencia a la fatiga of 580 - 685 MPa | 10⁸ cycles R=0 (Unidirectional) |
Resistencia a la tracción | 23.0 °C | 950 - 1090 MPa Show Supplier Material materials with Resistencia a la tracción of 950 - 1090 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1030 °C Show Supplier Material materials with Temperatura de fusión of 1030 °C |
Eléctrico
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 44 % IACS Show Supplier Material materials with Specific Electrical conductivity of 44 % IACS | nominal value |
Chemical properties
Property | Value |
---|---|
Berilio | 0.15 - 0.5 % Show Supplier Material materials with Berilio of 0.15 - 0.5 % |
Cobre | Balance |
Níquel | 1 - 1.4 % Show Supplier Material materials with Níquel of 1 - 1.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include power contacts and burn-in and test socket contacts. |