Medidas
Property | Value | Comment |
---|---|---|
Ancho | 610 mm Show Supplier Material materials with Ancho of 610 mm | max. |
Espesor | 0.5 - 6.25 mm Show Supplier Material materials with Espesor of 0.5 - 6.25 mm | |
Longitud | 1830 mm Show Supplier Material materials with Longitud of 1830 mm | max. |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 345 MPa |
Resistencia a la tracción | 23.0 °C | 483 MPa Show Supplier Material materials with Resistencia a la tracción of 483 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.16 % Show Supplier Material materials with Aluminio of 0.16 % | max. |
Berilio | 98 % Show Supplier Material materials with Berilio of 98 % | min., BeO: 2% max |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Hierro | 0.18 % Show Supplier Material materials with Hierro of 0.18 % | max. |
Magnesio | 0.08 % Show Supplier Material materials with Magnesio of 0.08 % | max. |
Otro | 0.04 % Show Supplier Material materials with Otro of 0.04 % | max., other metallic impurities each |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Intelligence, surveillance and reconnaissance (ISR) systems, Electro-optical infrared (EO/IR) & targeting systems, Airborne early warning & control systems (AEW&C), Surveillance, reconnaissance and targeting (SRT), Size, weight and power (SWaP) replacement systems, Semiconductor capital equipment, Space-based systems and components, James Webb Space Telescope support structure | |
Processing history | The standard condition of sheet shall be hot rolled, ground, stress relieved and etched. Rework of local areas may be performed within tolerances established by this specification. Surface finish shall be 63 microinches rms or finer. |