General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 23.0 °C | 1.85 g/cm³ Show Supplier Material materials with Densidad aparente of 1.85 g/cm³ | for BeO amount of 0.9% |
Tamaño de grano | 15 μm Show Supplier Material materials with Tamaño de grano of 15 μm | max. |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % |
Límite elástico Rp 0,2 | 23.0 °C | 207 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 207 MPa |
Resistencia a la tracción | 23.0 °C | 345 MPa Show Supplier Material materials with Resistencia a la tracción of 345 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.05 % Show Supplier Material materials with Aluminio of 0.05 % | max. |
Berilio | 99.2 % Show Supplier Material materials with Berilio of 99.2 % | min., BeO: 0.9% max |
Calcio | 5E-3 % Show Supplier Material materials with Calcio of 5E-3 % | max. |
Carbono | 0.09 % Show Supplier Material materials with Carbono of 0.09 % | max. |
Circonio | 0.03 % Show Supplier Material materials with Circonio of 0.03 % | max. |
Cobalto | 5E-3 % Show Supplier Material materials with Cobalto of 5E-3 % | max. |
Cobre | 0.03 % Show Supplier Material materials with Cobre of 0.03 % | max. |
Cromo | 0.01 % Show Supplier Material materials with Cromo of 0.01 % | max. |
Hierro | 0.08 % Show Supplier Material materials with Hierro of 0.08 % | max. |
Magnesio | 0.01 % Show Supplier Material materials with Magnesio of 0.01 % | max. |
Manganeso | 5E-3 % Show Supplier Material materials with Manganeso of 5E-3 % | max. |
Molibdeno | 5E-3 % Show Supplier Material materials with Molibdeno of 5E-3 % | max. |
Níquel | 0.03 % Show Supplier Material materials with Níquel of 0.03 % | max. |
Otro | 0.04 % Show Supplier Material materials with Otro of 0.04 % | max., other metallic impurities each |
Plata | 5E-3 % Show Supplier Material materials with Plata of 5E-3 % | max. |
Plomo | 5E-3 % Show Supplier Material materials with Plomo of 5E-3 % | max. |
Silicona | 0.05 % Show Supplier Material materials with Silicona of 0.05 % | max. |
Titanio | 0.03 % Show Supplier Material materials with Titanio of 0.03 % | max. |
Uranio | 0.02 % Show Supplier Material materials with Uranio of 0.02 % | max. |
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for nuclear test reactors and fusion walls due to their neutron reflectivity, neutron kinetic energy absorption, neutron kinetic energy absorption and high purity. Other applications are: Neutron reflectors and moderators, Neutron filter assemblies, Nuclear test reactors and Medical isotope reactors | |
Processing history | Hot isostatic pressing |