General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9 g/cm³ Show Supplier Material materials with Densidad of 9 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 41 - 203 mm Show Supplier Material materials with Diámetro of 41 - 203 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.33 [-] |
Dureza Rockwell C | 23.0 °C | 22 [-] Show Supplier Material materials with Dureza Rockwell C of 22 [-] |
Elongación | 23.0 °C | 12 - 15 % Show Supplier Material materials with Elongación of 12 - 15 % |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 620 MPa |
Módulo elástico | 23.0 °C | 144 GPa Show Supplier Material materials with Módulo elástico of 144 GPa |
Resistencia a la tracción | 23.0 °C | 760 MPa Show Supplier Material materials with Resistencia a la tracción of 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.64E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K |
Conductividad térmica | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Conductividad térmica of 38 W/(m·K) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad eléctrica | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 4.00E+6 S/m | max. |
Specific Electrical conductivity | 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS | max. |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | ToughMet 3 AT alloy is used for bushings and bearings for commercial aircraft, high performance engines as well as mining, industrial and heavy equipment. It is also used to make oil and gas drilling hardware, including rotary steerable housings, kelly valve seats and pressure housings. | |
Surface Finish | Mill hardened finish |