General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9 g/cm³ Show Supplier Material materials with Densidad of 9 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Diámetro | 6.35 - 10 mm Show Supplier Material materials with Diámetro of 6.35 - 10 mm | also for less than 6.35mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.33 [-] | |
Dureza Rockwell C | 23.0 °C | 32 [-] Show Supplier Material materials with Dureza Rockwell C of 32 [-] | |
Elongación | 23.0 °C | 5 - 7 % Show Supplier Material materials with Elongación of 5 - 7 % | in 4D |
Límite elástico Rp 0,2 | 23.0 °C | 1035 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 1035 MPa | |
Módulo elástico | 23.0 °C | 144 GPa Show Supplier Material materials with Módulo elástico of 144 GPa | |
Resistencia a la tracción | 23.0 °C | 1105 MPa Show Supplier Material materials with Resistencia a la tracción of 1105 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.64E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K |
Conductividad térmica | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Conductividad térmica of 38 W/(m·K) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad eléctrica | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 4.00E+6 S/m | max. |
Specific Electrical conductivity | 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS | max. |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | ToughMet 3 TS alloy tempers are commonly used in the oil and gas industry, oil & gas production via our sucker rod couplings and in commercial aircraft. |