General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9 g/cm³ Show Supplier Material materials with Densidad of 9 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro exterior | 28.6 - 254 mm Show Supplier Material materials with Diámetro exterior of 28.6 - 254 mm |
Diámetro interior | 12.7 - 76.2 mm Show Supplier Material materials with Diámetro interior of 12.7 - 76.2 mm |
Wall thickness | 6.35 - 15.9 mm Show Supplier Material materials with Wall thickness of 6.35 - 15.9 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-] | |
Dureza Rockwell C | 23.0 °C | 27 [-] Show Supplier Material materials with Dureza Rockwell C of 27 [-] | |
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | |
Límite elástico Rp 0,2 | 23.0 °C | 621 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 621 MPa | |
Módulo elástico | 23.0 °C | 144 GPa Show Supplier Material materials with Módulo elástico of 144 GPa | |
Resistencia a la fatiga | 23.0 °C | 413 MPa Show Supplier Material materials with Resistencia a la fatiga of 413 MPa | 10⁶ cycles R=-1 |
Resistencia a la tracción | 23.0 °C | 724 MPa Show Supplier Material materials with Resistencia a la tracción of 724 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Conductividad térmica of 38 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 9 % IACS Show Supplier Material materials with Specific Electrical conductivity of 9 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | ToughMet 3 CX alloy is used for wear plates, bushings, sleeve bearings, linear bearings and thrust bearings in industrial, off-road, mining and heavy equipment. It is also used for oil and gas drilling hardware. |