General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.17 g/cm³ Show Supplier Material materials with Densidad of 2.17 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.15 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.15 [-] | |
Compressive yield strength | 23.0 °C | 147 MPa Show Supplier Material materials with Compressive yield strength of 147 MPa | |
Elongación | 23.0 °C | 4.7 % Show Supplier Material materials with Elongación of 4.7 % | |
Límite elástico Rp 0,2 | 23.0 °C | 147.5 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 147.5 MPa | |
Módulo elástico | 23.0 °C | 193 GPa Show Supplier Material materials with Módulo elástico of 193 GPa | |
Resistencia a la fatiga | 23.0 °C | 86.2 MPa Show Supplier Material materials with Resistencia a la fatiga of 86.2 MPa | 10⁷ cycles, R=-1, Kt=1 |
Resistencia a la tracción | 23.0 °C | 196.5 MPa Show Supplier Material materials with Resistencia a la tracción of 196.5 MPa | |
Resistencia al cizallamiento | 23.0 °C | 181 MPa Show Supplier Material materials with Resistencia al cizallamiento of 181 MPa | Pin Double Shear Strength |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 1560 J/(kg·K) Show Supplier Material materials with Calor específico of 1560 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.46E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.46E-5 1/K |
Conductividad térmica | 23.0 °C | 110 W/(m·K) Show Supplier Material materials with Conductividad térmica of 110 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 48 % IACS Show Supplier Material materials with Specific Electrical conductivity of 48 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Berilio | 56 - 68 % Show Supplier Material materials with Berilio of 56 - 68 % | ||
Cobalto | 0.2 % Show Supplier Material materials with Cobalto of 0.2 % | max | |
Germanio | 0.2 % Show Supplier Material materials with Germanio of 0.2 % | max. | |
Hierro | 0.45 % Show Supplier Material materials with Hierro of 0.45 % | max. | |
Níquel | 2.4 - 3.5 % Show Supplier Material materials with Níquel of 2.4 - 3.5 % | ||
Plata | 0.2 % Show Supplier Material materials with Plata of 0.2 % | max. | |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % | max. |
Technological properties
Property |
---|