General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.17 g/cm³ Show Supplier Material materials with Densidad of 2.17 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.2 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.2 [-] | |
Compressive yield strength | 23.0 °C | 226.1 MPa Show Supplier Material materials with Compressive yield strength of 226.1 MPa | |
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | |
Límite elástico Rp 0,2 | 23.0 °C | 213.7 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 213.7 MPa | |
Módulo elástico | 23.0 °C | 193 GPa Show Supplier Material materials with Módulo elástico of 193 GPa | |
Resistencia a la fatiga | 23.0 °C | 117.2 MPa Show Supplier Material materials with Resistencia a la fatiga of 117.2 MPa | 10⁷ cycles, R=-1, Kt=1 |
Resistencia a la tracción | 23.0 °C | 289.6 MPa Show Supplier Material materials with Resistencia a la tracción of 289.6 MPa | |
Resistencia al cizallamiento | 23.0 °C | 247.5 MPa Show Supplier Material materials with Resistencia al cizallamiento of 247.5 MPa | Pin Double Shear Strength |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 1250 J/(kg·K) Show Supplier Material materials with Calor específico of 1250 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.42E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.42E-5 1/K |
Conductividad térmica | 23.0 °C | 105.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 105.5 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 40 % IACS Show Supplier Material materials with Specific Electrical conductivity of 40 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Berilio | 61.1 - 68.6 % Show Supplier Material materials with Berilio of 61.1 - 68.6 % | ||
Cobalto | 0.65 - 1.35 % Show Supplier Material materials with Cobalto of 0.65 - 1.35 % | ||
Germanio | 0.55 - 0.95 % Show Supplier Material materials with Germanio of 0.55 - 0.95 % | ||
Hierro | 0.45 % Show Supplier Material materials with Hierro of 0.45 % | max. | |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | max. | |
Plata | 2.65 - 3.35 % Show Supplier Material materials with Plata of 2.65 - 3.35 % | ||
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % | max. |
Technological properties
Property |
---|