General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Densidad of 8.83 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 1.27 - 406.5 mm Show Supplier Material materials with Ancho of 1.27 - 406.5 mm | |
Espesor | 0.05 - 0.38 mm Show Supplier Material materials with Espesor of 0.05 - 0.38 mm | thinner gauges maybe available upon request |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 300 [-] Show Supplier Material materials with Dureza Vickers of 300 [-] | |
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | for strip thicker than 0.10 mm |
Límite elástico Rp 0,2 | 23.0 °C | 951 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 951 MPa | |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 1 - 3.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 - 3.5 [-] | depending on the thickness |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 1 - 3.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 - 3.5 [-] | depending on the thickness |
Resistencia a la fatiga | 23.0 °C | 552 MPa Show Supplier Material materials with Resistencia a la fatiga of 552 MPa | 10⁷ cycles, R=0 |
Resistencia a la tracción | 23.0 °C | 986 MPa Show Supplier Material materials with Resistencia a la tracción of 986 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 419 J/(kg·K) Show Supplier Material materials with Calor específico of 419 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 208 W/(m·K) Show Supplier Material materials with Conductividad térmica of 208 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 42 % IACS Show Supplier Material materials with Specific Electrical conductivity of 42 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Excellent material for production sockets, appliance switches, relays, sensors and controls. |