General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.88 g/cm³ Show Supplier Material materials with Densidad of 8.88 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 0.76 - 15.8 mm Show Supplier Material materials with Diámetro of 0.76 - 15.8 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 4 - 30 % Show Supplier Material materials with Elongación of 4 - 30 % |
Límite elástico Rp 0,2 | 23.0 °C | 380 - 660 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 380 - 660 MPa |
Resistencia a la tracción | 23.0 °C | 480 - 720 MPa Show Supplier Material materials with Resistencia a la tracción of 480 - 720 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.77E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K |
Conductividad térmica | 23.0 °C | 210 W/(m·K) Show Supplier Material materials with Conductividad térmica of 210 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.90E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.90E+7 S/m |
Specific Electrical conductivity | 50 % IACS Show Supplier Material materials with Specific Electrical conductivity of 50 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Fósforo | 0.15 - 0.35 % Show Supplier Material materials with Fósforo of 0.15 - 0.35 % |
Níquel | 0.8 - 1.2 % Show Supplier Material materials with Níquel of 0.8 - 1.2 % |
Plomo | 0.8 - 1.2 % Show Supplier Material materials with Plomo of 0.8 - 1.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Brush 1916 is a strong material to machine or form into electrical contacts, connector pins and sockets. | |
General machinability | The addition of lead in the Brush 1915 & Brush 1916 alloy composition allows for chip control in turning and drilling operations, making the alloy ideal for automatic machining. Brush 1915 & Brush 1916 machines readily at feeds and speeds used for other leaded copper alloys. High speed steel and carbide tools are recommended for all machining operations. |