General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Densidad of 8.36 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 12 - 13 % Show Supplier Material materials with Elongación of 12 - 13 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 620 - 760 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 620 - 760 MPa | min. |
Módulo elástico | 23.0 °C | 131 GPa Show Supplier Material materials with Módulo elástico of 131 GPa | |
Resistencia a la tracción | 23.0 °C | 830 - 970 MPa Show Supplier Material materials with Resistencia a la tracción of 830 - 970 MPa | min. |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Conductividad térmica of 105 W/(m·K) |
Temperatura de fusión | 870 °C Show Supplier Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.8E-6 - 6.9E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.8E-6 - 6.9E-6 Ω·m |
Specific Electrical conductivity | 25 - 30 % IACS Show Supplier Material materials with Specific Electrical conductivity of 25 - 30 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Berilio | 1.8 - 2 % Show Supplier Material materials with Berilio of 1.8 - 2 % | ||
Cobalto | 0.2 % Show Supplier Material materials with Cobalto of 0.2 % | min. Nickel + Cobalt | |
Cobre | Balance | ||
Hierro | 0.6 % Show Supplier Material materials with Hierro of 0.6 % | max., Nickel + Cobalt + Iron | |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | min. Nickel + Cobalt | |
Plomo | 0.2 - 0.6 % Show Supplier Material materials with Plomo of 0.2 - 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration. |