General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Densidad of 8.36 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 1.27 - 2 mm Show Supplier Material materials with Diámetro of 1.27 - 2 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 - 8 % Show Supplier Material materials with Elongación of 2 - 8 % |
Límite elástico Rp 0,2 | 23.0 °C | 790 - 1040 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 790 - 1040 MPa |
Módulo elástico | 23.0 °C | 131 GPa Show Supplier Material materials with Módulo elástico of 131 GPa |
Resistencia a la tracción | 23.0 °C | 890 - 1070 MPa Show Supplier Material materials with Resistencia a la tracción of 890 - 1070 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Conductividad térmica of 105 W/(m·K) |
Temperatura de fusión | 870 °C Show Supplier Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 6.2E-6 - 7.8E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 6.2E-6 - 7.8E-6 Ω·m |
Specific Electrical conductivity | 22 - 28 % IACS Show Supplier Material materials with Specific Electrical conductivity of 22 - 28 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Berilio | 1.8 - 2 % Show Supplier Material materials with Berilio of 1.8 - 2 % | ||
Cobalto | 0.2 % Show Supplier Material materials with Cobalto of 0.2 % | min. Nickel + Cobalt | |
Cobre | Balance | ||
Hierro | 0.6 % Show Supplier Material materials with Hierro of 0.6 % | max., Nickel + Cobalt + Iron | |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | min. Nickel + Cobalt |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames. |