General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.5 g/cm³ Show Supplier Material materials with Densidad of 7.5 g/cm³ |
Medidas
Property | Value | Comment | |
---|---|---|---|
Diámetro exterior | 406 mm Show Supplier Material materials with Diámetro exterior of 406 mm | max. | |
Longitud | contact the supplier | ||
Wall thickness | Nominally 10-20% of OD |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % |
Límite elástico Rp 0,2 | 23.0 °C | 621 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 621 MPa |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa |
Resistencia a la tracción | 23.0 °C | 862 MPa Show Supplier Material materials with Resistencia a la tracción of 862 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 23.0 °C | 42 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42 W/(m·K) |
Temperatura de fusión | 1040 °C Show Supplier Material materials with Temperatura de fusión of 1040 °C |
Eléctrico
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.1 - 1.2 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.1 - 1.2 [-] |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 10.5 - 11.5 % Show Supplier Material materials with Aluminio of 10.5 - 11.5 % | |
Cobre | 74.5 % Show Supplier Material materials with Cobre of 74.5 % | |
Estaño | 0.25 % Show Supplier Material materials with Estaño of 0.25 % | max. |
Hierro | 4 - 5.5 % Show Supplier Material materials with Hierro of 4 - 5.5 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 4.2 - 6 % Show Supplier Material materials with Níquel of 4.2 - 6 % | |
Zinc | 0.3 % Show Supplier Material materials with Zinc of 0.3 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. They are also commonly used for applications in the oil & gas and other durable goods markets. |