General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.86 g/cm³ Show Supplier Material materials with Densidad of 1.86 g/cm³ | Theoretical density for BeO: 2.2% |
Tamaño de grano | 15 μm Show Supplier Material materials with Tamaño de grano of 15 μm | max., ASTM E-112 |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 1 - 2 % Show Supplier Material materials with Elongación of 1 - 2 % |
Límite elástico Rp 0,2 | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 345 MPa |
Resistencia a la tracción | 23.0 °C | 448 MPa Show Supplier Material materials with Resistencia a la tracción of 448 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 % Show Supplier Material materials with Aluminio of 0.1 % | max. |
Berilio | 98 % Show Supplier Material materials with Berilio of 98 % | min., BeO: 2.2% max |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Hierro | 0.15 % Show Supplier Material materials with Hierro of 0.15 % | max. |
Magnesio | 0.08 % Show Supplier Material materials with Magnesio of 0.08 % | max. |
Otro | 0.04 % Show Supplier Material materials with Otro of 0.04 % | max., other metallic impurities each |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It is hot isostatically pressed beryllium grades used in space applications and for low-density, bare polished optical applications or when reduced weight is required. |