General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.81 g/cm³ Show Supplier Material materials with Densidad of 8.81 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 0.15 - 0.8 mm Show Supplier Material materials with Espesor of 0.15 - 0.8 mm | gauge |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-] | |
Dureza Vickers | 23.0 °C | 160 - 200 [-] Show Supplier Material materials with Dureza Vickers of 160 - 200 [-] | |
Elongación | 23.0 °C | 5 - 10 % Show Supplier Material materials with Elongación of 5 - 10 % | for strip thicker than 0.10 mm |
Límite elástico Rp 0,2 | 23.0 °C | 550 - 580 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 550 - 580 MPa | |
Módulo elástico | 23.0 °C | 137 - 152 GPa Show Supplier Material materials with Módulo elástico of 137 - 152 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 0.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0.5 [-] | |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 0.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0.5 [-] | |
Resistencia a la tracción | 23.0 °C | 613 - 648 MPa Show Supplier Material materials with Resistencia a la tracción of 613 - 648 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 210 W/(m·K) Show Supplier Material materials with Conductividad térmica of 210 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.90E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.90E+7 S/m |
Specific Electrical conductivity | 48 - 50 % IACS Show Supplier Material materials with Specific Electrical conductivity of 48 - 50 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Cobre | 99.5 % Show Supplier Material materials with Cobre of 99.5 % | min. |
Cromo | 0.5 - 3 % Show Supplier Material materials with Cromo of 0.5 - 3 % | Ni+Si+Cr |
Níquel | 0.5 - 3 % Show Supplier Material materials with Níquel of 0.5 - 3 % | Ni+Si+Cr |
Silicona | 0.5 - 3 % Show Supplier Material materials with Silicona of 0.5 - 3 % | Ni+Si+Cr |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Wire Harness Terminals and High Voltage Connectors, EV Charging Contacts, Appliance Power Contacts, Computer Power Contacts, Backplane, Midplane and Card Edge Connectors, Photovoltaic System Connectors, Heat Spreading for Consumer Electronics |