General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 30 [-] Show Supplier Material materials with Dureza Rockwell C of 30 [-] | |
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | |
Energía de impacto Charpy | 23.0 °C | 20 J Show Supplier Material materials with Energía de impacto Charpy of 20 J | |
Límite elástico Rp 0,2 | 23.0 °C | 720 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 720 MPa | |
Módulo elástico | 23.0 °C | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa | |
Resistencia a la fatiga | 23.0 °C | 240 MPa Show Supplier Material materials with Resistencia a la fatiga of 240 MPa | 10⁷ cycles, R=-1 |
Resistencia a la tracción | 23.0 °C | 790 MPa Show Supplier Material materials with Resistencia a la tracción of 790 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 100.0 °C | 390 J/(kg·K) Show Supplier Material materials with Calor específico of 390 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Conductividad térmica | 100.0 °C | 70 W/(m·K) Show Supplier Material materials with Conductividad térmica of 70 W/(m·K) |
Temperatura de fusión | 925 °C Show Supplier Material materials with Temperatura de fusión of 925 °C |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Estaño | 5.5 - 6.5 % Show Supplier Material materials with Estaño of 5.5 - 6.5 % |
Níquel | 8.5 - 9.5 % Show Supplier Material materials with Níquel of 8.5 - 9.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | MoldMAX XL Alloy is used as injection mold cores and cavities. |