General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.69 g/cm³ Show Supplier Material materials with Densidad of 8.69 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 12.5 - 63.5 mm Show Supplier Material materials with Diámetro of 12.5 - 63.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 250 - 265 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 250 - 265 [-] | |
Dureza Rockwell C | 23.0 °C | 25 - 27 [-] Show Supplier Material materials with Dureza Rockwell C of 25 - 27 [-] | HRC values converted per ASTM-E-140, Table 1. |
Elongación | 23.0 °C | 5 - 7 % Show Supplier Material materials with Elongación of 5 - 7 % | |
Energía de impacto Charpy | 23.0 °C | 7 J Show Supplier Material materials with Energía de impacto Charpy of 7 J | |
Límite elástico Rp 0,2 | 23.0 °C | 690 - 790 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 690 - 790 MPa | |
Módulo elástico | 23.0 °C | 130 GPa Show Supplier Material materials with Módulo elástico of 130 GPa | |
Resistencia a la fatiga | 23.0 °C | 275 MPa Show Supplier Material materials with Resistencia a la fatiga of 275 MPa | 10⁷ cycles, R=-1 |
Resistencia a la tracción | 23.0 °C | 790 - 860 MPa Show Supplier Material materials with Resistencia a la tracción of 790 - 860 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 100.0 °C | 410 J/(kg·K) Show Supplier Material materials with Calor específico of 410 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 100.0 °C | 160 W/(m·K) Show Supplier Material materials with Conductividad térmica of 160 W/(m·K) |
Temperatura de fusión | 980 °C Show Supplier Material materials with Temperatura de fusión of 980 °C |
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Cromo | 0.6 - 1.2 % Show Supplier Material materials with Cromo of 0.6 - 1.2 % |
Níquel | 6.4 - 7.6 % Show Supplier Material materials with Níquel of 6.4 - 7.6 % |
Silicona | 1.5 - 2.5 % Show Supplier Material materials with Silicona of 1.5 - 2.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Applications include injection mold and blow mold cores and cavities. |