General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Densidad of 8.83 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1.27 - 452.7 mm Show Supplier Material materials with Ancho of 1.27 - 452.7 mm |
Espesor | 0.05 - 3.18 mm Show Supplier Material materials with Espesor of 0.05 - 3.18 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 216 - 287 [-] Show Supplier Material materials with Dureza Vickers of 216 - 287 [-] | |
Elongación | 23.0 °C | 8 - 20 % Show Supplier Material materials with Elongación of 8 - 20 % | for strip with 0.1mm and thicker. |
Límite elástico Rp 0,2 | 23.0 °C | 650 - 830 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 650 - 830 MPa | |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | for strip with 0.25mm and thinner. |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 1 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | for strip with 0.25mm and thinner. |
Resistencia a la tracción | 23.0 °C | 750 - 940 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 940 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 240 W/(m·K) Show Supplier Material materials with Conductividad térmica of 240 W/(m·K) |
Temperatura de fusión | 1040 °C Show Supplier Material materials with Temperatura de fusión of 1040 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.9E-6 - 3.8E-6 Ω·m |
Specific Electrical conductivity | 45 - 60 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 0.2 - 0.6 % Show Supplier Material materials with Berilio of 0.2 - 0.6 % |
Cobre | Balance |
Níquel | 1.4 - 2.2 % Show Supplier Material materials with Níquel of 1.4 - 2.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability spring contacts for switches and relays. |