General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Densidad of 8.83 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro exterior | 9.5 - 76 mm Show Supplier Material materials with Diámetro exterior of 9.5 - 76 mm |
Wall thickness | Typically 10 to 20% of OD |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 23.0 °C | 92 [-] Show Supplier Material materials with Dureza Rockwell B of 92 [-] |
Elongación | 20.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % |
427.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | |
Límite elástico Rp 0,2 | 20.0 °C | 585 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 585 MPa |
427.0 °C | 450 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 450 MPa | |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa |
Resistencia a la tracción | 20.0 °C | 690 MPa Show Supplier Material materials with Resistencia a la tracción of 690 MPa |
427.0 °C | 515 MPa Show Supplier Material materials with Resistencia a la tracción of 515 MPa | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 414 J/(kg·K) Show Supplier Material materials with Calor específico of 414 J/(kg·K) | at 25°C |
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K | |
Conductividad térmica | 23.0 °C | 225 W/(m·K) Show Supplier Material materials with Conductividad térmica of 225 W/(m·K) | at 25°C |
Temperatura de fusión | 1010 °C Show Supplier Material materials with Temperatura de fusión of 1010 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.6E-6 - 3.2E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.6E-6 - 3.2E-6 Ω·m |
Specific Electrical conductivity | 45 - 55 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 55 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 0.4 - 0.7 % Show Supplier Material materials with Berilio of 0.4 - 0.7 % |
Circonio | 0.12 - 0.4 % Show Supplier Material materials with Circonio of 0.12 - 0.4 % |
Cobalto | 2 - 2.7 % Show Supplier Material materials with Cobalto of 2 - 2.7 % |
Cobre | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | High performance powertrain automotive applications such as exhaust valve seats. |