General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Densidad of 8.83 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 305 - 559 mm Show Supplier Material materials with Ancho of 305 - 559 mm |
Espesor | 4.8 - 76 mm Show Supplier Material materials with Espesor of 4.8 - 76 mm |
Longitud | 610 - 3200 mm Show Supplier Material materials with Longitud of 610 - 3200 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 - 8 % Show Supplier Material materials with Elongación of 2 - 8 % |
Límite elástico Rp 0,2 | 23.0 °C | 380 - 550 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 380 - 550 MPa |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa |
Resistencia a la tracción | 23.0 °C | 480 - 590 MPa Show Supplier Material materials with Resistencia a la tracción of 480 - 590 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Conductividad térmica of 200 W/(m·K) |
Temperatura de fusión | 1010 °C Show Supplier Material materials with Temperatura de fusión of 1010 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.9E-6 - 3.8E-6 Ω·m |
Specific Electrical conductivity | 45 - 60 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 0.4 - 0.7 % Show Supplier Material materials with Berilio of 0.4 - 0.7 % |
Cobalto | 2.4 - 2.7 % Show Supplier Material materials with Cobalto of 2.4 - 2.7 % |
Cobre | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding. |