General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1.27 - 406.5 mm Show Supplier Material materials with Ancho of 1.27 - 406.5 mm |
Espesor | 0.05 - 2 mm Show Supplier Material materials with Espesor of 0.05 - 2 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 180 - 230 [-] Show Supplier Material materials with Dureza Vickers of 180 - 230 [-] | |
Elongación | 23.0 °C | 10 - 20 % Show Supplier Material materials with Elongación of 10 - 20 % | |
Límite elástico Rp 0,2 | 23.0 °C | 550 - 690 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 550 - 690 MPa | |
Módulo elástico | 23.0 °C | 138 GPa Show Supplier Material materials with Módulo elástico of 138 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 0.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0.5 [-] | for strip with 0.25mm and thinner. |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 0.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0.5 [-] | for strip with 0.25mm and thinner. |
Resistencia a la fatiga | 23.0 °C | 515 - 585 MPa Show Supplier Material materials with Resistencia a la fatiga of 515 - 585 MPa | 10⁸ cycles R=0 (Unidirectional) |
Resistencia a la tracción | 23.0 °C | 665 - 790 MPa Show Supplier Material materials with Resistencia a la tracción of 665 - 790 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 230 W/(m·K) Show Supplier Material materials with Conductividad térmica of 230 W/(m·K) |
Temperatura de fusión | 1020 °C Show Supplier Material materials with Temperatura de fusión of 1020 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.9E-6 - 3.8E-6 Ω·m |
Specific Electrical conductivity | 45 - 60 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 60 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 0.15 - 0.5 % Show Supplier Material materials with Berilio of 0.15 - 0.5 % |
Cobalto | 0.35 - 0.6 % Show Supplier Material materials with Cobalto of 0.35 - 0.6 % |
Cobre | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability automotive terminals and spring contacts for switches and relays. |