General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.36 g/cm³ Show Supplier Material materials with Densidad of 8.36 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1.27 - 406.5 mm Show Supplier Material materials with Ancho of 1.27 - 406.5 mm |
Espesor | 0.03 - 0.05 mm Show Supplier Material materials with Espesor of 0.03 - 0.05 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 325 [-] Show Supplier Material materials with Dureza Vickers of 325 [-] | min. |
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 1103 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 1103 MPa | min. |
Módulo elástico | 23.0 °C | 131 GPa Show Supplier Material materials with Módulo elástico of 131 GPa | |
Resistencia a la tracción | 23.0 °C | 1200 MPa Show Supplier Material materials with Resistencia a la tracción of 1200 MPa | min. |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Conductividad térmica of 105 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 6.2E-6 - 1.01E-5 Ω·m Show Supplier Material materials with Resistividad eléctrica of 6.2E-6 - 1.01E-5 Ω·m |
Specific Electrical conductivity | 17 - 28 % IACS Show Supplier Material materials with Specific Electrical conductivity of 17 - 28 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Technological properties
Property | ||
---|---|---|
Application areas | EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. |