General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | |
Absorción de agua, saturación | 23.0 °C | 0.01 % Show Supplier Material materials with Absorción de agua, saturación of 0.01 % | max., DIN 53715, till 96h |
Coefficient of friction | 0.2 [-] Show Supplier Material materials with Coefficient of friction of 0.2 [-] | ||
Coefficient of friction, kinetic | 0.2 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.2 [-] | against steel (0.25m/s, 0.25N/mm) | |
Densidad | 23.0 °C | 0.94 g/cm³ Show Supplier Material materials with Densidad of 0.94 g/cm³ | max., DIN 53479, ISO 1183 |
Masa molar | 5.00E+6 g/mol Show Supplier Material materials with Masa molar of 5.00E+6 g/mol | ||
Moisture absorption | 23.0 °C | 0 % Show Supplier Material materials with Moisture absorption of 0 % | no moisture absorption |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 61 - 65 [-] Show Supplier Material materials with Dureza Shore D of 61 - 65 [-] | DIN 868, ISO 7619-1 |
Elongación | 23.0 °C | 300 % Show Supplier Material materials with Elongación of 300 % | min., DIN 53455, ISO 527-2 |
Hardness, Ball Indentation | 23.0 °C | 30 MPa Show Supplier Material materials with Hardness, Ball Indentation of 30 MPa | min., DIN 53456, ISO 2039 |
Límite elástico | 23.0 °C | 20 MPa Show Supplier Material materials with Límite elástico of 20 MPa | DIN 53455, ISO 527-2 |
Módulo elástico | 23.0 °C | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | min., DIN 53457, ISO 527-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 170 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 170 kJ/m² | min., DIN 53453, ISO 179 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2E-4 1/K | |||
Conductividad térmica | 23.0 °C | 0.4 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.4 W/(m·K) | DIN 52612 | ||
Heat deflection temperature, 1.80 MPa | 42 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 42 °C | ISO 75-A | |||
Temperatura de flexión bajo carga | 42 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 42 °C | ||||
Temperatura de fusión | 130 - 135 °C Show Supplier Material materials with Temperatura de fusión of 130 - 135 °C | ISO 3146 method C | |||
Temperatura máx. de funcionamiento | 80 - 90 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 80 - 90 °C | ||||
Temperatura máx. de funcionamiento, continuo | 80 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, continuo of 80 °C | DIN 53446, in air for 20000h | |||
Temperatura máx. de funcionamiento, corto | 90 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, corto of 90 °C | in air | |||
Temperatura mín. de funcionamiento | -200 °C Show Supplier Material materials with Temperatura mín. de funcionamiento of -200 °C | ||||
Inflamabilidad | UL94: HB, for 3/6mm |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1000000 Ω/sq Show Supplier Material materials with Surface resistivity of 1000000 Ω/sq | max., DIN 53482, ISO 60093 |
Volume resistivity | 23.0 °C | 1000000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000000 Ω·cm | max., DIN 53482, ISO 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean room technology, medical technology, electrical engineering, laboratory environment, chain guides Conveyor: Conveyor elements, Conveyor troughs, Conveyor slide lining, Conveyors stars, Antistatic sliding elements, Curved tracks, Curve guides, Conveyor belts Sliding: Sliding rails, Sliding profiles, Sliding segments Other applications: Wiping strips, Feed hooper, Outlets, Belt stripping, Bins, Gaskets, Format sets, Guiding elements, Sliding elements, Plain bearing, Link belts, Highly wear-resistant sliding elements, Chain guides, Sprockets, Crane support plates, Bearing bushes, Baffle plates, Moulding stripes, Pump parts, Belt guides, Rolls, Chain-pulled conveyors, Control discs, Transport chutes, Deflections pulleys, Wear bars, Workpiece carriers, Toothed wheels, Centrifuges | |
Certifications | Food Contact EU: No, FDA:No and ATEX 95 | |
Color | Light Grey AST | |
Wear resistance | Sand Slurry Test: 120% ISO 15527 |