General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 93 N Show Supplier Material materials with Adhesion of 93 N | min., Hot U Test |
Densidad lineal | 23.0 °C | 3.75E-3 - 4.55E-3 g/cm Show Supplier Material materials with Densidad lineal of 3.75E-3 - 4.55E-3 g/cm |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 60 mm Show Supplier Material materials with Bobbin Inner Diameter of 60 mm | |
Bobbin Length | 356 mm Show Supplier Material materials with Bobbin Length of 356 mm | |
Diámetro | 0.43 - 0.63 mm Show Supplier Material materials with Diámetro of 0.43 - 0.63 mm | Apparent Diameter |
Flange Diameter | 190.5 mm Show Supplier Material materials with Flange Diameter of 190.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.9 - 3.1 % Show Supplier Material materials with Elongación of 1.9 - 3.1 % | |
Nominal breaking force | 23.0 °C | 196 N Show Supplier Material materials with Nominal breaking force of 196 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.1/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 106 - 130 TPM | Direction: S & Z |