General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 125 N Show Supplier Material materials with Adhesion of 125 N | min., Hot U Test |
Densidad lineal | 23.0 °C | 0.03 - 0.04 g/cm Show Supplier Material materials with Densidad lineal of 0.03 - 0.04 g/cm |
Medidas
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 1600 N Show Supplier Material materials with Nominal breaking force of 1600 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.2/4 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 34 - 46 TPM | Direction: S & Z |