Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 667 N Show Supplier Material materials with Nominal breaking force of 667 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 330.3/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 19 to 28% | |
Twist per Meter | 52 - 68 TPM | Direction: S |