General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 50 N Show Supplier Material materials with Adhesion of 50 N | min., Hot U Test |
Densidad lineal | 23.0 °C | 7.5E-4 - 8.5E-4 g/cm Show Supplier Material materials with Densidad lineal of 7.5E-4 - 8.5E-4 g/cm |
Medidas
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 50 N Show Supplier Material materials with Nominal breaking force of 50 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Brown | |
Cord Construction | 68.1/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: SBR, Dip Pick-Up: 17 to 25% | |
Twist per Meter | 52 - 68 TPM | Direction: Z |