Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Chopped Strand G99-003007
NBR latex impregnated carbon fibre chopped strand (Elastomer Polymer Matrix Composite)
Los datos sobre este material han sido proporcionados por NGF Glass.
All categories
General
Property | Temperature | Value |
---|---|---|
Densidad lineal | 23.0 °C | 0.01 g/cm Show Supplier Material materials with Densidad lineal of 0.01 g/cm |
Medidas
Property | Value | Comment |
---|---|---|
Longitud | 2 - 6 mm Show Supplier Material materials with Longitud of 2 - 6 mm | Chopped Strand |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: NBR, Dip Pick-Up: 20 to 30% |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.