General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 343 N Show Supplier Material materials with Adhesion of 343 N | min., T Test |
Densidad lineal | 23.0 °C | 0.06 - 0.07 g/cm Show Supplier Material materials with Densidad lineal of 0.06 - 0.07 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 22 % Show Supplier Material materials with Loss on Ignition of 16 - 22 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Diámetro | 2.32 - 2.62 mm Show Supplier Material materials with Diámetro of 2.32 - 2.62 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.2 - 4.2 % Show Supplier Material materials with Elongación of 2.2 - 4.2 % | |
Nominal breaking force | 23.0 °C | 2453 N Show Supplier Material materials with Nominal breaking force of 2453 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 140.3/12 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 28 - 51 TPM | Direction: S & Z |