General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 120 N Show Supplier Material materials with Adhesion of 120 N | min., T Test |
Densidad lineal | 23.0 °C | 3.85E-3 - 4.25E-3 g/cm Show Supplier Material materials with Densidad lineal of 3.85E-3 - 4.25E-3 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 21 % Show Supplier Material materials with Loss on Ignition of 16 - 21 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 60 mm Show Supplier Material materials with Bobbin Inner Diameter of 60 mm | |
Bobbin Length | 360 mm Show Supplier Material materials with Bobbin Length of 360 mm | |
Diámetro | 0.45 - 0.65 mm Show Supplier Material materials with Diámetro of 0.45 - 0.65 mm | Apparent Diameter |
Flange Diameter | 139 mm Show Supplier Material materials with Flange Diameter of 139 mm |
Mecánica
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 110.1/3 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 124 - 160 TPM | Direction: S & Z |