Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 30 N Show Supplier Material materials with Adhesion of 30 N | min., T Test |
Densidad lineal | 23.0 °C | 1.05E-3 - 1.55E-3 g/cm Show Supplier Material materials with Densidad lineal of 1.05E-3 - 1.55E-3 g/cm | |
Loss on Ignition | 23.0 °C | 15 - 23 % Show Supplier Material materials with Loss on Ignition of 15 - 23 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 64 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 64 mm | tapered |
Bobbin Length | 305 mm Show Supplier Material materials with Bobbin Length of 305 mm | |
Diámetro | 0.28 - 0.38 mm Show Supplier Material materials with Diámetro of 0.28 - 0.38 mm | Apparent Diameter |
Flange Diameter | 152.5 mm Show Supplier Material materials with Flange Diameter of 152.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 50 N Show Supplier Material materials with Nominal breaking force of 50 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 34.3/0 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 130 - 154 TPM | Direction: S & Z |