General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 59 N Show Supplier Material materials with Adhesion of 59 N | min., T Test |
Densidad lineal | 23.0 °C | 1.2E-3 - 1.5E-3 g/cm Show Supplier Material materials with Densidad lineal of 1.2E-3 - 1.5E-3 g/cm | |
Loss on Ignition | 23.0 °C | 16.2 - 22.2 % Show Supplier Material materials with Loss on Ignition of 16.2 - 22.2 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 60 mm Show Supplier Material materials with Bobbin Inner Diameter of 60 mm | |
Bobbin Length | 360 mm Show Supplier Material materials with Bobbin Length of 360 mm | |
Diámetro | 0.26 - 0.4 mm Show Supplier Material materials with Diámetro of 0.26 - 0.4 mm | Apparent Diameter |
Flange Diameter | 139 mm Show Supplier Material materials with Flange Diameter of 139 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.7 - 3.7 % Show Supplier Material materials with Elongación of 1.7 - 3.7 % | |
Nominal breaking force | 23.0 °C | 59 N Show Supplier Material materials with Nominal breaking force of 59 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Cord Construction | 34.3/0 | |
Other | Manufacturing Location: UK / Poland | |
Processing history | Latex Type: Chloroprene | |
Twist per Meter | 130 - 154 TPM | Direction: S & Z |