General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 55 N Show Supplier Material materials with Adhesion of 55 N | min., T Test |
Densidad lineal | 23.0 °C | 1.25E-3 - 1.55E-3 g/cm Show Supplier Material materials with Densidad lineal of 1.25E-3 - 1.55E-3 g/cm | |
Loss on Ignition | 23.0 °C | 18 - 26 % Show Supplier Material materials with Loss on Ignition of 18 - 26 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Diámetro | 0.25 - 0.45 mm Show Supplier Material materials with Diámetro of 0.25 - 0.45 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.8 - 3.8 % Show Supplier Material materials with Elongación of 1.8 - 3.8 % | |
Nominal breaking force | 23.0 °C | 59 N Show Supplier Material materials with Nominal breaking force of 59 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Black Overcoat | |
Cord Construction | 110.1/0 | |
Other | Manufacturing Location: UK | |
Processing history | Latex Type: HNBR | |
Twist per Meter | 130 - 154 TPM | Direction: S & Z |