General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 100 N Show Supplier Material materials with Adhesion of 100 N | min., T Test |
Densidad lineal | 23.0 °C | 7.85E-3 - 8.95E-3 g/cm Show Supplier Material materials with Densidad lineal of 7.85E-3 - 8.95E-3 g/cm | |
Loss on Ignition | 23.0 °C | 16 - 25 % Show Supplier Material materials with Loss on Ignition of 16 - 25 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Diámetro | 0.76 - 0.96 mm Show Supplier Material materials with Diámetro of 0.76 - 0.96 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mecánica
Technological properties
Property | ||
---|---|---|
Color | Black Overcoat | |
Cord Construction | 110.1/6 | |
Other | Manufacturing Location: UK | |
Processing history | Latex Type: HNBR | |
Twist per Meter | 71 - 95 TPM | Direction: S & Z |