General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 130 N Show Supplier Material materials with Adhesion of 130 N | min., Peel |
Densidad lineal | 23.0 °C | 0.02 g/cm Show Supplier Material materials with Densidad lineal of 0.02 g/cm | |
Loss on Ignition | 23.0 °C | 21.5 - 26.5 % Show Supplier Material materials with Loss on Ignition of 21.5 - 26.5 % |
Medidas
Property | Value | Comment |
---|---|---|
Bobbin Inner Diameter | 57 - 63 mm Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm | tapered |
Bobbin Length | 341 mm Show Supplier Material materials with Bobbin Length of 341 mm | |
Diámetro | 1.05 - 1.25 mm Show Supplier Material materials with Diámetro of 1.05 - 1.25 mm | Apparent Diameter |
Flange Diameter | 279.5 mm Show Supplier Material materials with Flange Diameter of 279.5 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 - 4.3 % Show Supplier Material materials with Elongación of 2.5 - 4.3 % | |
Nominal breaking force | 23.0 °C | 1200 N Show Supplier Material materials with Nominal breaking force of 1200 N | Tensile Member: High Tensile K Glass |
Technological properties
Property | ||
---|---|---|
Color | Black Overcoat | |
Cord Construction | 22.8/18 | |
Other | Manufacturing Location: UK | |
Processing history | Latex Type: HNBR | |
Twist per Meter | 64 - 80 TPM | Direction: S & Z |