General
Property | Temperature | Value |
---|---|---|
Densidad lineal | 23.0 °C | 2.2E-4 - 6.8E-4 g/cm Show Supplier Material materials with Densidad lineal of 2.2E-4 - 6.8E-4 g/cm |
Loss on Ignition | 23.0 °C | 0.95 - 1.35 % Show Supplier Material materials with Loss on Ignition of 0.95 - 1.35 % |
Medidas
Property | Value |
---|---|
Bobbin Length | 280 mm Show Supplier Material materials with Bobbin Length of 280 mm |
Mecánica
Property | Value |
---|---|
Nominal breaking force | Tensile Member: U Glass |
Technological properties
Property | ||
---|---|---|
Color | White | |
Cord Construction | Yarn | |
Other | Manufacturing Location: Japan | |
Processing history | Latex Type: Plastic Size | |
Twist per Meter | 40 TPM | Direction: S & Z |