General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 680 Kg Show Supplier Material materials with Bonding strength of 680 Kg | ASTM D229 | Condition D-48/50 |
726 Kg Show Supplier Material materials with Bonding strength of 726 Kg | ASTM D229 | Condition A | |
Densidad | 1.95 g/cm³ Show Supplier Material materials with Densidad of 1.95 g/cm³ | ASTM D792 | |
Moisture absorption | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 115 [-] Show Supplier Material materials with Dureza Rockwell M of 115 [-] | ASTM D785 | |
Impact strength, Izod notched, ASTM | 598 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 598 J/m | ASTM D256 | Condition A, Transverse |
790 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 790 J/m | ASTM D256 | Condition A | |
Módulo de flexión | 21.4 GPa Show Supplier Material materials with Módulo de flexión of 21.4 GPa | ASTM D790 | Condition A, Transverse |
22.8 GPa Show Supplier Material materials with Módulo de flexión of 22.8 GPa | ASTM D790 | Condition A | |
Resistencia a la compresión | 482.6 MPa Show Supplier Material materials with Resistencia a la compresión of 482.6 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 317.6 MPa Show Supplier Material materials with Resistencia a la flexión of 317.6 MPa | Condition E-1/150: T-150, Transverse | |
351.6 MPa Show Supplier Material materials with Resistencia a la flexión of 351.6 MPa | ASTM D790 | Condition E-1/150: T-150 | |
358.5 MPa Show Supplier Material materials with Resistencia a la flexión of 358.5 MPa | Condition A, Transverse | ||
420.6 MPa Show Supplier Material materials with Resistencia a la flexión of 420.6 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 282.7 MPa Show Supplier Material materials with Resistencia a la tracción of 282.7 MPa | ASTM D638 | Condition A |
Resistencia al cizallamiento | 268.9 MPa Show Supplier Material materials with Resistencia al cizallamiento of 268.9 MPa | ASTM D732 | Transverse |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | ¹ | |
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | ¹ | |
Temperatura de transición del vidrio | 190 °C Show Supplier Material materials with Temperatura de transición del vidrio of 190 °C | DMA | |
Inflamabilidad | UL 94, Class V-1 |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 5.02 [-] Show Supplier Material materials with Constante dieléctrica of 5.02 [-] | 1MHz | ASTM D150 | Condition D₁24/23 |
Factor de disipación | 0.018 [-] Show Supplier Material materials with Factor de disipación of 0.018 [-] | 1MHz | ASTM D150 | Condition D₁24/23 |
Rigidez dieléctrica | 7.87 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 7.87 kV/mm | ASTM D149 | Condition A | |
Tensión de ruptura | 60 kV Show Supplier Material materials with Tensión de ruptura of 60 kV | ASTM D149 | Condition D-48/50 | |
70 kV Show Supplier Material materials with Tensión de ruptura of 70 kV | ASTM D149 | Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include structural applications when used in elevated temperatures. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |