General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1134 Kg Show Supplier Material materials with Bonding strength of 1134 Kg | ASTM D229 | Condition A |
Densidad | 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | ASTM D792 | |
Moisture absorption | 0.22 % Show Supplier Material materials with Moisture absorption of 0.22 % | ASTM D570 | Condition A |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 99 [-] Show Supplier Material materials with Dureza Rockwell M of 99 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 400 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 400 J/m | ASTM D256 | Condition E-48/50, Transverse |
507 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 507 J/m | ASTM D256 | Condition E-48/50 | |
Módulo de flexión | 22.8 GPa Show Supplier Material materials with Módulo de flexión of 22.8 GPa | ASTM D790 | Condition A, Transverse |
23.4 GPa Show Supplier Material materials with Módulo de flexión of 23.4 GPa | ASTM D790 | Condition A | |
Resistencia a la compresión | 433 MPa Show Supplier Material materials with Resistencia a la compresión of 433 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 413.7 MPa Show Supplier Material materials with Resistencia a la flexión of 413.7 MPa | ASTM D790 | Condition A, Transverse |
455.1 MPa Show Supplier Material materials with Resistencia a la flexión of 455.1 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 296.5 MPa Show Supplier Material materials with Resistencia a la tracción of 296.5 MPa | ASTM D638 | Condition A |
Resistencia al cizallamiento | 131 MPa Show Supplier Material materials with Resistencia al cizallamiento of 131 MPa | ASTM D732 | Condition A, Transverse |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9.6e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.6e-06 1/K | IPC-TM 650-2.4.24 | Transverse | ||
1.21e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.21e-05 1/K | IPC-TM 650-2.4.24 | ||||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL Bulletin 746b¹ | |||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL Bulletin 746b¹ | |||
Temperatura de transición del vidrio | 120 °C Show Supplier Material materials with Temperatura de transición del vidrio of 120 °C | DMA | |||
Inflamabilidad | UL Bulletin 94, Class HB |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Rigidez dieléctrica | 27.17 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 27.17 kV/mm | ASTM D149 | Condition A & D-48/50 |
Tensión de ruptura | 48 kV Show Supplier Material materials with Tensión de ruptura of 48 kV | ASTM D149 | Condition A |
49 kV Show Supplier Material materials with Tensión de ruptura of 49 kV | ASTM D149 | Condition D-48/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Applications for NP500A include: low temperature thermal insulation, structural applications and various other mechanical, and electrical applications at low to moderately high temperatures. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |