General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 1.86 g/cm³ Show Supplier Material materials with Densidad of 1.86 g/cm³ | ASTM D792 | |
Moisture absorption | 0.14 % Show Supplier Material materials with Moisture absorption of 0.14 % | ASTM D570 | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 105 [-] Show Supplier Material materials with Dureza Rockwell M of 105 [-] | ASTM D785 | |
Módulo de compresión | 4.8 GPa Show Supplier Material materials with Módulo de compresión of 4.8 GPa | ASTM D695 | Condition A |
Resistencia a la compresión | 206.8 MPa Show Supplier Material materials with Resistencia a la compresión of 206.8 MPa | ASTM D638 | Condition E-1/150: T-150 |
241.3 MPa Show Supplier Material materials with Resistencia a la compresión of 241.3 MPa | ASTM D638 | Condition A | |
Resistencia a la tracción | 220.6 MPa Show Supplier Material materials with Resistencia a la tracción of 220.6 MPa | ASTM D638 | Condition E-1/150: T-150 |
268.9 MPa Show Supplier Material materials with Resistencia a la tracción of 268.9 MPa | ASTM D638 | Condition A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 200 °C Show Supplier Material materials with Relative temperature index, electrical of 200 °C | ¹ | |
Relative temperature index, mechanical strength | 200 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 200 °C | ¹ | |
Temperatura de transición del vidrio | 170 °C Show Supplier Material materials with Temperatura de transición del vidrio of 170 °C | min. | DMA | |
Inflamabilidad | UL Bulletin 94, Class HB |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.39 [-] Show Supplier Material materials with Constante dieléctrica of 4.39 [-] | 1MHz | ASTM D150 | Condition A |
4.62 [-] Show Supplier Material materials with Constante dieléctrica of 4.62 [-] | 1MHz | ASTM D150 | Condition D-24/23 | |
4.62 [-] Show Supplier Material materials with Constante dieléctrica of 4.62 [-] | 1MHz | ASTM D150 | Condition D-48/50 | |
Factor de disipación | 0.024 [-] Show Supplier Material materials with Factor de disipación of 0.024 [-] | 1MHz | ASTM D150 | Condition A |
0.034 [-] Show Supplier Material materials with Factor de disipación of 0.034 [-] | 1MHz | ASTM D150 | Condition D-24/23 | |
0.04 [-] Show Supplier Material materials with Factor de disipación of 0.04 [-] | 1MHz | ASTM D150 | Condition D-48/50 | |
Rigidez dieléctrica | 14.96 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 14.96 kV/mm | ASTM D149 | Condition D-48/50 | |
15.74 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15.74 kV/mm | ASTM D149 | Condition A | ||
Tensión de ruptura | 55 kV Show Supplier Material materials with Tensión de ruptura of 55 kV | ASTM D149 | Condition A | |
70 kV Show Supplier Material materials with Tensión de ruptura of 70 kV | ASTM D149 | Condition D-48/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include bushings, spacers and structural parts for power generation equipment. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |