General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 1.79 g/cm³ Show Supplier Material materials with Densidad of 1.79 g/cm³ | ASTM D349 | |
Moisture absorption | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | ASTM D349 | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 110 [-] Show Supplier Material materials with Dureza Rockwell M of 110 [-] | ASTM D349 | |
Resistencia a la compresión | 468.8 MPa Show Supplier Material materials with Resistencia a la compresión of 468.8 MPa | ASTM D349 | Condition A |
Resistencia a la flexión | 411.6 MPa Show Supplier Material materials with Resistencia a la flexión of 411.6 MPa | ASTM D349 | Condition A |
Resistencia a la tracción | 255.1 MPa Show Supplier Material materials with Resistencia a la tracción of 255.1 MPa | ASTM D349 | Condition A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | ¹ | |
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | ¹ | |
Inflamabilidad | UL 94, Class HB |
Technological properties
Property | ||
---|---|---|
Application areas | It can and is used as a substitute for silicon glass materials in many applications. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |