General
Property | Value | Comment |
---|---|---|
Bonding strength | 725.74 Kg Show Supplier Material materials with Bonding strength of 725.74 Kg | Condition A |
Densidad | 1.89 g/cm³ Show Supplier Material materials with Densidad of 1.89 g/cm³ | |
Moisture absorption | 0.56 % Show Supplier Material materials with Moisture absorption of 0.56 % |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell M | 112 [-] Show Supplier Material materials with Dureza Rockwell M of 112 [-] | |
Impact strength, Izod notched, ASTM | 453.7 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 453.7 J/m | Transverse |
731.3 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 731.3 J/m | ||
Resistencia a la compresión | 526.8 MPa Show Supplier Material materials with Resistencia a la compresión of 526.8 MPa | Flatwise |
Resistencia a la flexión | 338.5 MPa Show Supplier Material materials with Resistencia a la flexión of 338.5 MPa | Transverse |
484.0 MPa Show Supplier Material materials with Resistencia a la flexión of 484.0 MPa | ||
Resistencia a la tracción | 378.5 MPa Show Supplier Material materials with Resistencia a la tracción of 378.5 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL 94, Class HB |
Technological properties
Property | ||
---|---|---|
Application areas | Insulating gaskets | |
Fillers | Glass Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |