General
Property | Value | Comment |
---|---|---|
Bonding strength | 816.46 Kg Show Supplier Material materials with Bonding strength of 816.46 Kg | Condition A |
Densidad | 1.89 g/cm³ Show Supplier Material materials with Densidad of 1.89 g/cm³ | |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | Condition D₁-24/23 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 108 [-] Show Supplier Material materials with Dureza Rockwell M of 108 [-] | ||
Impact strength, Izod notched, ASTM | 549.8 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 549.8 J/m | Condition E-48/50, Transverse | |
667.2 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 667.2 J/m | Condition E-48/50 | ||
Resistencia a la compresión | 497.1 MPa Show Supplier Material materials with Resistencia a la compresión of 497.1 MPa | Condition A | Flatwise | |
Resistencia a la flexión | 289 MPa Show Supplier Material materials with Resistencia a la flexión of 289 MPa | ASTM D790 | Condition E-1/150: T-150, Transverse |
315 MPa Show Supplier Material materials with Resistencia a la flexión of 315 MPa | ASTM D790 | Condition E-1/150: T-150 | |
365.4 MPa Show Supplier Material materials with Resistencia a la flexión of 365.4 MPa | ASTM D790 | Condition A, Transverse | |
472.3 MPa Show Supplier Material materials with Resistencia a la flexión of 472.3 MPa | ASTM D790 | Condition A | |
Resistencia a la tracción | 326.1 MPa Show Supplier Material materials with Resistencia a la tracción of 326.1 MPa | ||
Resistencia al cizallamiento | 173.7 MPa Show Supplier Material materials with Resistencia al cizallamiento of 173.7 MPa | Transverse |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de transición del vidrio | 180 °C Show Supplier Material materials with Temperatura de transición del vidrio of 180 °C | min. | DMA | |
Arc resistance | 185 seconds, ASTM D495, Condition A | ||
Inflamabilidad | UL 94, Class V-0 |
Eléctrico
Property | Value | Frequency | Comment |
---|---|---|---|
Constante dieléctrica | 4.1 [-] Show Supplier Material materials with Constante dieléctrica of 4.1 [-] | 1MHz | Condition D₁-24/23 |
Factor de disipación | 0.018 [-] Show Supplier Material materials with Factor de disipación of 0.018 [-] | 1MHz | Condition D-24/23 |
Rigidez dieléctrica | 26.77 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26.77 kV/mm | Condition D-48/50 | |
29.92 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 29.92 kV/mm | Condition A | ||
Tensión de ruptura | 69 kV Show Supplier Material materials with Tensión de ruptura of 69 kV | Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include electrical equipment subjected to elevated temperatures. | |
Fillers | Glass Fabric | |
Other | The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |