General
Property | Value | Comment |
---|---|---|
Bonding strength | 997.9 Kg Show Supplier Material materials with Bonding strength of 997.9 Kg | Condition A |
Densidad | 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.8 g/cm³ | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | Condition D₁-24/23 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell M | 100 [-] Show Supplier Material materials with Dureza Rockwell M of 100 [-] | |
Impact strength, Izod notched, ASTM | 640.5 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 640.5 J/m | Condition E-48/50, Transverse |
747.3 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 747.3 J/m | Condition E-48/50 | |
Módulo de flexión | 16.5 GPa Show Supplier Material materials with Módulo de flexión of 16.5 GPa | Condition A, Transverse |
18.6 GPa Show Supplier Material materials with Módulo de flexión of 18.6 GPa | Condition A | |
Resistencia a la compresión | 448.2 MPa Show Supplier Material materials with Resistencia a la compresión of 448.2 MPa | Condition A | Flatwise |
Resistencia a la flexión | 517.1 MPa Show Supplier Material materials with Resistencia a la flexión of 517.1 MPa | Condition A |
65000 MPa Show Supplier Material materials with Resistencia a la flexión of 65000 MPa | Condition A, Transverse | |
Resistencia a la tracción | 310.3 MPa Show Supplier Material materials with Resistencia a la tracción of 310.3 MPa | Condition A |
Resistencia al cizallamiento | 151.7 MPa Show Supplier Material materials with Resistencia al cizallamiento of 151.7 MPa | Transverse |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Coeficiente de dilatación térmica | 1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-05 1/K | ||
1.3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.3e-05 1/K | Transverse | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | ¹ | |
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | ¹ | |
Temperatura de transición del vidrio | 115 °C Show Supplier Material materials with Temperatura de transición del vidrio of 115 °C | ||
Arc resistance | 100 seconds, Condition A | ||
Inflamabilidad | UL 94, Class HB |
Eléctrico
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.8 [-] Show Supplier Material materials with Constante dieléctrica of 4.8 [-] | 1MHz | Condition D₁-24/23 | |
Factor de disipación | 0.025 [-] Show Supplier Material materials with Factor de disipación of 0.025 [-] | 1MHz | Condition D₁-24/23 | |
Rigidez dieléctrica | 25.98 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25.98 kV/mm | Condition D-48/50 | ||
26.37 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26.37 kV/mm | Condition A | |||
Tensión de ruptura | 50 kV Show Supplier Material materials with Tensión de ruptura of 50 kV | ASTM D149 | Condition D-48/50 | |
60 kV Show Supplier Material materials with Tensión de ruptura of 60 kV | ASTM D149 | Condition A | ||
Índice de seguimiento comparativo | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V |
Technological properties
Property | ||
---|---|---|
Application areas | It is used in cryogenic applications. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |