General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1134 Kg Show Supplier Material materials with Bonding strength of 1134 Kg | ASTM D229 | Condition A |
Densidad | 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.8 g/cm³ | ASTM D792 | |
Moisture absorption | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ASTM D570 | Condition A |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 110 [-] Show Supplier Material materials with Dureza Rockwell M of 110 [-] | ASTM D785 | |
Impact strength, Izod unnotched, ASTM | 641 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 641 J/m | ASTM D256 | Condition E-48/50 |
Resistencia a la compresión | 351.6 MPa Show Supplier Material materials with Resistencia a la compresión of 351.6 MPa | ASTM D695 | Condition A | Flatwise |
Resistencia a la flexión | 434.4 MPa Show Supplier Material materials with Resistencia a la flexión of 434.4 MPa | ASTM D790 | Condition A |
Resistencia a la tracción | 317.2 MPa Show Supplier Material materials with Resistencia a la tracción of 317.2 MPa | ASTM D790 | Condition A |
Resistencia al cizallamiento | 151.7 MPa Show Supplier Material materials with Resistencia al cizallamiento of 151.7 MPa | ASTM D732 | Condition A, Transverse |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL Bulletin 746b¹ | |
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL Bulletin 746b¹ | |
Inflamabilidad | UL Bulletin 94, Class HB |
Eléctrico
Property | Value | Testing Standard |
---|---|---|
Surface resistivity | 100000 - 1e+09 Ω/sq Show Supplier Material materials with Surface resistivity of 100000 - 1e+09 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | This material is used where static dissipation is required from surfaces to surface of the composite, in the x, y and z directions. | |
Fillers | Glass Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |