General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Bonding strength | 1043.26 Kg Show Supplier Material materials with Bonding strength of 1043.26 Kg | ASTM D229 | Condition D-48/50 |
1133.98 Kg Show Supplier Material materials with Bonding strength of 1133.98 Kg | ASTM D229 | Condition A | |
Densidad | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | ||
Moisture absorption | 3.5 % Show Supplier Material materials with Moisture absorption of 3.5 % | Condition D₁-24/23 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell M | 100 [-] Show Supplier Material materials with Dureza Rockwell M of 100 [-] | |
Impact strength, Izod unnotched, ASTM | 175 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 175 J/m | Condition E-48/50, Transverse |
195 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 195 J/m | Condition E-48/50 | |
Módulo de flexión | 10.3 GPa Show Supplier Material materials with Módulo de flexión of 10.3 GPa | Condition A, Transverse |
11.0 GPa Show Supplier Material materials with Módulo de flexión of 11.0 GPa | Condition A | |
Resistencia a la compresión | 234.4 MPa Show Supplier Material materials with Resistencia a la compresión of 234.4 MPa | Condition A |
Resistencia a la flexión | 117.2 MPa Show Supplier Material materials with Resistencia a la flexión of 117.2 MPa | Condition A, Transverse |
126.9 MPa Show Supplier Material materials with Resistencia a la flexión of 126.9 MPa | Condition A | |
Resistencia a la tracción | 82.7 MPa Show Supplier Material materials with Resistencia a la tracción of 82.7 MPa | Condition A |
Resistencia al cizallamiento | 96.5 MPa Show Supplier Material materials with Resistencia al cizallamiento of 96.5 MPa | Transverse |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-05 1/K | IPC-TM 650-2.4.24 | |||
2.2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | IPC-TM 650-2.4.24 | Transverse | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | ¹ | |||
Arc resistance | 15 seconds, ASTM D495, Condition A | ||||
Inflamabilidad | UL 94, Class HB, Condition A |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Rigidez dieléctrica | 5.91 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 5.91 kV/mm | Condition D48/50 | |
15.75 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15.75 kV/mm | Condition A | ||
Tensión de ruptura | 5 kV Show Supplier Material materials with Tensión de ruptura of 5 kV | Condition D48/50 | |
20 kV Show Supplier Material materials with Tensión de ruptura of 20 kV | Condition A | ||
Índice de seguimiento comparativo | 155 V Show Supplier Material materials with Índice de seguimiento comparativo of 155 V | ASTM D3638 |
Technological properties
Property | ||
---|---|---|
Application areas | Applications include spacers for installation of liquid oxygen apparatus where temperatures are as low as minus 320 F. | |
Fillers | Cotton Fabric | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |