Phenolic BT12NPN - Tube

Nombres alternativos y comerciales
U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

Fine weave canvas phenolic material with fabric construction weight intermediate to BT13NPN and BT25NPN. BT12NPN is designed for better machining than grade BT13NPN and lower cost than BT25NPN.

Los datos sobre este material han sido proporcionados por Norplex Micarta.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyValueTesting StandardComment

Densidad

1.3 g/cm³

Show Supplier Material materials with Densidad of 1.3 g/cm³

ASTM D792

Moisture absorption

1.8 %

Show Supplier Material materials with Moisture absorption of 1.8 %

ASTM D570

Condition D₁-24/23

Mecánica

PropertyValueTesting StandardComment

Dureza Rockwell M

100 [-]

Show Supplier Material materials with Dureza Rockwell M of 100 [-]

ASTM D785

Módulo de compresión

2.2 GPa

Show Supplier Material materials with Módulo de compresión of 2.2 GPa

ASTM D695

Condition A

Resistencia a la compresión

179.3 MPa

Show Supplier Material materials with Resistencia a la compresión of 179.3 MPa

ASTM D695

Condition A

Resistencia a la tracción

51.7 MPa

Show Supplier Material materials with Resistencia a la tracción of 51.7 MPa

ASTM D638

Condition A

Aplicaciones térmicas

PropertyValueComment

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

¹

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

¹

Inflamabilidad

UL Bulletin 94, Class HB, Condition A

Eléctrico

PropertyValueTesting StandardComment

Rigidez dieléctrica

7.48 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 7.48 kV/mm

ASTM D149

Condition A

Technological properties

Property
Fillers

Cotton Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use


2.The mechanical properties are converted from American unit system to International unit system.

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".