General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D348 |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | ASTM D348 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Rockwell M | 74 [-] Show Supplier Material materials with Dureza Rockwell M of 74 [-] | ASTM D348 | |
Módulo de compresión | 2.5 GPa Show Supplier Material materials with Módulo de compresión of 2.5 GPa | ASTM D348 | Condition A |
Resistencia a la compresión | 151.7 MPa Show Supplier Material materials with Resistencia a la compresión of 151.7 MPa | ASTM D348 | Condition A |
Resistencia a la tracción | 28.3 MPa Show Supplier Material materials with Resistencia a la tracción of 28.3 MPa | ASTM D348 | Condition A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | ¹ | |
Inflamabilidad | UL Bulletin 94, Class HB, Condition A |
Technological properties
Property | ||
---|---|---|
Application areas | BT18NPA is designed for highly loaded bearing applications, where the lubrication is provided by oil, water or a mixture. | |
Fillers | Cotton Fabric and Alumina | |
Other | 1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use 2.The mechanical properties are converted from American unit system to International unit system. | |
Supplier Disclaimer | This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values". To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest. It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available. |